pipeline and oil tube weld crack corrosion detection
1.Portable Metal Corrosion Detectors
2. metal detector
3. pipe test
Port: Xiamen
Minimum Order Quantity: 3 Set/Sets Samples are available
Supply Ability: 200 Set/Sets per Month
Payment Terms: T/T
Contact SupplierPackaging Detail: Packed in a special water-proof case
Delivery Detail: According to your minimum order quantity
pipeline and oil tube weld crack corrosion detection
1.Portable Metal Corrosion Detectors
2. metal detector
3.metal pipe detect
Model | IDEA-1502 |
Product | Metal Corrosion Testing Instrument |
Type | Eddy Current |
Description | Metal corrosion detector is designed for the steel tubes corrosion testing. It is distinguished for its high-resolution colorful LCD, adjustable phase, gain and testing frequency, and applicable to various metal corrosion detecting. The English and Chinese operation interface makes it more intuitive and easier for operation |
Specification | 1. Large screen, high-luminance color LCD display 2. Fast digital / analog electronic balance 3. Easy to operate, real-time on-screen instruction |
Parameter | 1. Separate testing channels: 2( to improve the testing efficiency) 2. Frequency range: 10 Hz~10 MHz, adjustable 3. Gain: 0 dB~99 dB,wide gain range 4. Phase: 0~359°,flexible phase rotation. 5. Testing speed: >60M/min, applicable to various testing speed requirements 6. The testing accuracy up to 0.01mm, with high testing accuracy. 7. Lift-off height: >3mm, no requirement of the surface clearness. 8. Phase/non-amplitude, box and fan box to meet different requirements. 9. Probe Drive: 1 ~ 8, to meet different probe structures, the true sense of the multi-functional 12. USB 2.0(Host)connection for output 13. eddy current testing signal playback, analysis, archiving, printing features 16. On-line hotkey graphics, text help. 17. Built-in rechargeable lithium battery 8000MAH |
Application | Applied to metal parts and tubes defects testing as structure, weld, crack and corrosion detecting. |