Er:Yag, Nd:YAG, Nd:YVO4,Cr:YAG Q-switch,
Laser Crystal
BBO
a-BBO
Port: China
Minimum Order Quantity: 1 Piece/Pieces
Supply Ability: 500 Piece/Pieces per Month
Payment Terms: L/C,D/P,T/T
Contact SupplierPackaging Detail: Box
Delivery Detail: 30 Dyas
ER:YAG
Er:YAG is an excellent laser crystal which lasers at 2.94μm.It has wide applications in medical laser systems, and others.
Advantages of Er:YAG Crystals
Material and Specifications
Dopant concentration | Er: ~50 at% |
Orientation | [111] within 5° |
Wavefront Distortion | ≤0.125λ/inch( at1064nm) |
Extinction Ratio | ≥25 dB |
Rod Sizes | Diameter:36mm, Length:50120 mm Upon request of customer |
Dimensional Tolerances | Diameter:+0.000"/-0.002", Length: ± 0.02" |
Barrel Finish | Ground Finish: 400# Grit |
Parallelism | ≤10" |
Perpendicularity | ≤5 |
Flatness | λ/10 |
Surface Quality | 10-5(MIL-O-13830A) |
Chamfer | 0.006"±0.002" |
AR Coating Reflectivity | ≤ 0.25% (at 2940nm) |
Laser Transition | 4I11/2to4I13/2 |
Laser Wavelength | 2940nm |
Photon Energy | 6.75×10-20J( at 2940nm) |
Emission Cross Section | 3×10-20cm2 |
Index of Refraction | 1.79 at 2940nm |
Pump Bands | 600~800 nm |
Crystal Structure | Cubic |
Lattice Parameters | 12.01 Å |
Melting Point | 1970 |
Moh Hardness | 8.5 |
Density | 4.56±0.04g/cm3 |
Specific Heat (0-20) | 0.59J/g.cm3 |
Modulus of Elasticity | 310GPa |
Young's Modulus | 3.17×104Kg/mm2 |
Poisson Ratio | 0.3(est.) |
Tensile Strength | 0.13~0.26GPa |
Thermal Expansion Coefficient | [100]Direction:8.2×10-6/(0~250) |
[110]Direction:7.7×10-6/(0~250) | |
[111]Direction:7.8×10-6/(0~250) | |
Thermal Conductivity | 14W/m/K(at 20) |
10.5W/m/K(at 100) | |
Thermal Optical Coefficient (dn/dT) | 7.3×10-6/ |
Thermal Shock Resistance | 790W/m |
Solubility | Water: Insoluble; Common Acids: Slightly |